Microfractography of alpha plutonium

Microfractography of alpha plutonium

4.11 - 1251 ratings - Source

The rods are then immersed in a FC-75 bath maintained at 20 C. The whole operation takes less than 5 sec. After ultrasonic agitation in FC-75 to remove particulate matter, the fracture interface is ready for replication. Replicas of the fractureanbsp;...

Title:Microfractography of alpha plutonium
Author:G. E. Miller, T. K. Bierlein, B. Mastel, U.S. Atomic Energy Commission, United States. Energy Research and Development Administration, U.S. Atomic Energy Commission. Research and Engineering Operation N-Reactor Department
Publisher: - 1964